Melting of Aluminum requires temperatures in the range of 647 degree Celsius and 757 degree Celsius.
Aging of aluminum alloy requires a temperature range of 122 degree Celsius to 237 degree Celsius.
Annealing of Aluminum alloy requires a temperature range of 232 degree Celsius to 412 degree Celsius.
Forging of Aluminum alloy is carried out in the temperature range of 343 degree Celsius to 521 degree Celsius.
Rolling of Aluminum alloy can be achieved if the furnace heat is at a temperature of 455 degree Celsius.
Stress relieving of Aluminum alloy is best achieved in the temperature range of 342 degree Celsius and 647 degree Celsius.
Annealing of Brass is best achieved in the temperature range of 317 degree Celsius and 538 degree Celsius.
Extruding of Brass is best achieved at a temperature range between 757 degree Celsius and 787 degree Celsius.
Forging of Brass happens best between a temperature range of 567 degree Celsius and 757 degree Celsius.
Rolling of Brass can be achieved at a temperature of 738 degree Celsius.
Sintering of Brass is achieved in the temperature range of 843 degree Celsius and 871 degree Celsius.
Red Brass has a melting temperature of 997 degree Celsius.
Yellow Brass has a melting temperature of 927 degree Celsius.
Sintering of Bronze is carried out in the temperature range between 760 degree Celsius and 871 degree Celsius.
It can be melted at 1057 degree Celsius.
It can be melted at 897 degree Celsius.
It can be melted at 1047 degree Celsius.
It can be melted at 887 degree Celsius.
Melting point of Cadmium is 322 degree Celsius.
Melting point of Calcium is 850 degree Celsius.
Melting point of Cobalt is 1490 degree Celsius.
Annealing of copper can be carried out in the temperature range between 427 degree Celsius and 647 degree Celsius.
Forging of copper can be carried out at a temperature of 982 degree Celsius.
Copper can be melted if the temperature is maintained between 1147 degree Celsius and 1257 degree Celsius.
Copper can be refined if the temperature is maintained between 1147 degree Celsius and 1427 degree Celsius.
Rolling of Copper can be achieved at a temperature of 871 degree Celsius.
Sintering of Copper can be achieved if the temperature is in the range of 843 degree Celsius and 899 degree Celsius.
Smelting of Copper requires a temperature range of 1147 degree Celsius and 1427 degree Celsius.
The melting of iron in a blast furnace happens in a temperature range of 1372 degree Celsius and 1537 degree Celsius.
The melting of iron in a cupola furnace happens in at a temperature range of 1427 degree Celsius and 1537 degree Celsius.
Annealing of cast iron requires a temperature range of 705 degree Celsius and 955 degree Celsius.
Austenitizing of cast iron requires a temperature range of 787 degree Celsius and 927 degree Celsius.
Malleablizing of cast iron requires a temperature range of 897 degree Celsius and 982 degree Celsius.
Melting of cast iron in a cupola furnace happens in the temperature range of 1427 degree Celsius and 1527 degree Celsius.
Normalizing of cast iron can be achieved in the temperature range of 872 degree Celsius and 937 degree Celsius.
Stress relieving of cast iron can be achieved in the temperature range of 427 degree Celsius and 672 degree Celsius.
Melting of malleable iron requires a temperature range of 1317 degree Celsius and 1707 degree Celsius.
Annealing of malleable iron using the long cycle requires a temperature range of 817 degree Celsius and 927 degree Celsius.
Annealing of malleable iron using the short cycle requires a temperature of 982 degree Celsius.
Sintering of iron requires a temperature range of 1577 degree Celsius and 1827 degree Celsius.
Annealing of steel requires a temperature range of 677 degree Celsius and 899 degree Celsius.
Austenitizing of steel requires a temperature range of 760 degree Celsius and 927 degree Celsius.
Bessemer converter needs heat in the range of 1537 degree Celsius and 1647 degree Celsius for steel production.
Calorizing of steel requires a temperature of 927 degree Celsius.
Carbonitriding of steel requires a temperature range of 505 degree Celsius and 899 degree Celsius.
Carburizing of steel requires a temperature of 1477 degree Celsius.
Case hardening of steel requires a temperature range of 867 degree Celsius and 927 degree Celsius.
Cyaniding of steel requires a temperature range of 757 degree Celsius and 977 degree Celsius.
Drawing forgings of steel requires a temperature of 452 degree Celsius.
Drop-forging of steel requires a temperature range of 1202 degree Celsius and 1317 degree Celsius.
Forging of steel requires a temperature range of 927 degree Celsius and 1177 degree Celsius.
Form-bending of steel requires a temperature range of 867 degree Celsius and 977 degree Celsius.
Galvanizing of steel requires a temperature range of 427 degree Celsius and 487 degree Celsius.
Heat treating of steel requires a temperature range of 377 degree Celsius and 977 degree Celsius.
Lead hardening of steel requires a temperature range of 757 degree Celsius and 977 degree Celsius.
Open hearth steel melting requires a temperature range of 1537 degree Celsius and 1702 degree Celsius.
Electric furnace melts steel in the temperature range of 1317 degree Celsius and 1757 degree Celsius.
Nitriding of steel requires a temperature range of 510 degree Celsius and 565 degree Celsius.
Normalizing of steel requires a temperature range of 897 degree Celsius and 1037 degree Celsius.
The temperature required for rolling steel is in the range of 1205 degree Celsius and 1260 degree Celsius.
Sintering of steel requires a temperature in the range of 1093 degree Celsius and 1288 degree Celsius.
Spheroidizing of steel requires a temperature range of 677 degree Celsius and 721 degree Celsius.
Stress relieving of steel requires a temperature range of 232 degree Celsius and 649 degree Celsius.
Tempering of steel for drawing requires a temperature range of 149 degree Celsius and 760 degree Celsius.